Customization: | Available |
---|---|
Material: | POM |
Kind: | Hard Plastic Rods |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Material | Brand | Size (Rod) | Services | Application |
POM 500P | MBH | Dia. 4 /5/6/7/8/9/10/13/16/18/22/ 25/26/40/45/50/55/60/65/70/75 /80/85/90/95/100/120/170/230/260 or customized |
sheet/rod/profile extrusion and machining |
medical, pharmaceutical, and semi-conductor, water treatment |
Delrin® 500P is a general purpose medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability, a good combination of mechanical properties, and low VOC emissions.
heological properties | Value | Unit | Test Standard |
Melt volume-flow rate, MVR | 13 | cm³/10min | ISO 1133 |
Temperature | 190 | °C | ISO 1133 |
Load | 2.16 | kg | ISO 1133 |
Molding shrinkage, parallel | 2.0 | % | ISO 294-4, 2577 |
Molding shrinkage, normal | 1.9 | % | ISO 294-4, 2577 |
Mechanical properties | Value | Unit | Test Standard |
Tensile modulus | 3100 | MPa | ISO 527-1/-2 |
Yield stress | 71 | MPa | ISO 527-1/-2 |
Yield strain | 17 | % | ISO 527-1/-2 |
Nominal strain at break | 30 | % | ISO 527-1/-2 |
Tensile creep modulus, 1h | 2800 | MPa | ISO 899-1 |
Tensile creep modulus, 1000h | 1600 | MPa | ISO 899-1 |
Charpy impact strength, +23°C | 300 | kJ/m² | ISO 179/1eU |
Charpy impact strength, -30°C | 280 | kJ/m² | ISO 179/1eU |
Charpy notched impact strength, +23°C | 9 | kJ/m² | ISO 179/1eA |
Charpy notched impact strength, -30°C | 8 | kJ/m² | ISO 179/1eA |
Puncture - maximum force, +23°C | 2000 | N | ISO 6603-2 |
Puncture energy, +23°C | 3 | J | ISO 6603-2 |
Thermal properties | Value | Unit | Test Standard |
Melting temperature, 10°C/min | 178 | °C | ISO 11357-1/-3 |
Temp. of deflection under load, 1.80 MPa | 93 | °C | ISO 75-1/-2 |
Temp. of deflection under load, 0.45 MPa | 160 | °C | ISO 75-1/-2 |
Vicat softening temperature, 50°C/h 50N | 155 | °C | ISO 306 |
Coeff. of linear therm. expansion, parallel | 100 | E-6/K | ISO 11359-1/-2 |
Coeff. of linear therm. expansion, normal | 100 | E-6/K | ISO 11359-1/-2 |
Burning behavior at 1.5 mm nominal thickness | HB | class | IEC 60695-11-10 |
Thickness tested (1.5) | 1.5 | mm | IEC 60695-11-10 |
Yellow Card available | Yes | - | - |
Burning behavior at thickness h | HB | class | IEC 60695-11-10 |
Thickness tested (h) | 0.8 | mm | IEC 60695-11-10 |
Yellow Card available | Yes | - | - |
Oxygen index | 22 | % | ISO 4589-1/-2 |
Electrical properties | Value | Unit | Test Standard |
Relative permittivity, 100Hz | 3.8 | - | IEC 62631-2-1 |
Relative permittivity, 1MHz | 3.8 | - | IEC 62631-2-1 |
Dissipation factor, 100Hz | 90 | E-4 | IEC 62631-2-1 |
Dissipation factor, 1MHz | 90 | E-4 | IEC 62631-2-1 |
Volume resistivity | 2E12 | Ohm*m | IEC 62631-3-1 |
Surface resistivity | 4E14 | Ohm | IEC 62631-3-2 |
Electric strength | 44 | kV/mm | IEC 60243-1 |
Comparative tracking index | 600 | - | IEC 60112 |
Other properties | Value | Unit | Test Standard |
Water absorption | 1.3 | % | Sim. to ISO 62 |
Humidity absorption | 0.2 | % | Sim. to ISO 62 |
Density | 1420 | kg/m³ | ISO 1183 |